The following thumbnail photos illustrate thermal images of electrical, process and roofing problems. Click on the thumbnail for enlargement of the image. Contact us for more details.

77s.jpg (4202 bytes) 78s.jpg (4150 bytes) 79s.jpg (4390 bytes) 80s.jpg (3692 bytes) 85s.jpg (4849 bytes)

1. infrared image of loose internal bushing on a transformer

2. real images of
internal bushing problem

3.  image of
loose connection

4. real images of
loose connection

5. infrared scan with Agema infrared camera

91s.jpg (4246 bytes) 92s.jpg (5675 bytes) 84s.jpg (6480 bytes) 112s.jpg (4354 bytes) 113s.jpg (5445 bytes)

6. image of wet insulation on a built up roof

7. image of wet insulation adjacent to a soil vent

8. verification of moisture content

9. infrared photo of a loose jumper connection 10. loose lug connection of a high voltage switch
114s.jpg (5491 bytes) 115s.jpg (5395 bytes) 116s.jpg (4819 bytes) 117s.jpg (5005 bytes) 118s.jpg (5459 bytes)

11. loose connection from a breaker to a fuse on both phases

12. first phase fuse top clip is loose 13. first phase fuse clip and bolts are loose on a breaker 14.  third phase fuse top clip and lug for disconnect is defective 15.  third phase fuse and lug connection on a breaker is loose
119s.jpg (3873 bytes) 120s.jpg (3664 bytes) 121s.jpg (3914 bytes) 122s.jpg (4217 bytes) 123s.jpg (3515 bytes)

16. transformer bushing connection is loose internally

17.  refractory lining on a rotating kiln is defective 18. defective 15 amp breaker found in a lighting panel 19. poor connection at the jaws of a switch 20. loose fuse holder on a high voltage fuse
124s.jpg (3670 bytes) 125s.jpg (3435 bytes) 126s.jpg (4105 bytes)

21. wet fibreboard insulation panel on a flat roof

22. wet insulation found adjacent to a roof drain 23. wet fibrous glass insulation panel found in a roof 24. electrical disconnect panel, thermal image of the 1st phase incoming lug connection found to be loose 25. evaluation of refractory lining in a process kiln furnace

26. evaluation of refractory lining for a process gas breaching

27. infrared image of defective refractory lining for process vessels and breaching 28. defective refractory lining for an incinerator 29. loose lug connection on a starter in an electrical panel 30. defective knife blades in an electrical disconnect

31. loose fuse clips in an electrical panel

32. loose lug connection at top of an electrical breaker 33.  defective elbow and bushing for a high voltage pad mount transformer 34. wet insulation found in a built up flat roof system. 35. loose lug connection on a high voltage switch

36.  defective high voltage switch

37. heat loss around access doors on a gas breaching 38.  refractory lining conditions for a process furnace and associated gas flue 39.  heat loss for a boiler side wall casing 40.  internal IR scan of a refinery process heater tubes

41. coke located on bottom tubes (light gray area) in a process refinery heater

For details contact: btessler@thermacoeng.com